There has to be no proof of cracking in the sample when it can be flattened amongst flat plates to no more than six (6) times the wall thickness. If this check fails, one particular added sample in the similar lot could be taken. If this next sample fails, the https://bar178rtp65532.thenerdsblog.com/32766622/bar-178-secrets